CERTAL® SPC, Al rolled plate

Want to keep this datasheet? Save it now in your required format

Description

Precision rolled plate UNIDAL® made form alloy EN AW 7019 (AlZn4Mg2), finely milled on both sides and covered with protective film, is characterized by a narrow tolerance of flatness and thickness and has only relatively low residual stresses. The good anodizing and welding capability opens up a wide range of applications for this product.

Equivalent Materials

This material data has been provided by Gleich Aluminum.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.76 g/cm³

Show Supplier Material materials with Density of 2.76 g/cm³

Dimension

PropertyValue

Dimensions

Standard stock sizes: 1020mm x 2020mm and 150-180mm in thickness (T651), 1520mm x 3020mm and 150-300mm in thickness (T652)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

72 GPa

Show Supplier Material materials with Elastic modulus of 72 GPa

Elongation A50

23.0 °C

2 - 7 %

Show Supplier Material materials with Elongation A50 of 2 - 7 %

Hardness, HBW

23.0 °C

140 - 160 [-]

Show Supplier Material materials with Hardness, HBW of 140 - 160 [-]

Test method: 2.5/62.5

Tensile strength

23.0 °C

490 - 530 MPa

Show Supplier Material materials with Tensile strength of 490 - 530 MPa

Yield strength Rp0.2

23.0 °C

430 - 460 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 430 - 460 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

2.36E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.36E-5 1/K

Specific heat capacity

23.0 °C

873 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 873 J/(kg·K)

Thermal conductivity

23.0 °C

120 - 150 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 120 - 150 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

1.80E+7 - 2.20E+7 S/m

Show Supplier Material materials with Electrical conductivity of 1.80E+7 - 2.20E+7 S/m

Technological properties

Property
Other

Heat treatable alloy

Processing history

Temper: T651, T652