G-3645UV (LLDPE)

Alternative and trade names
G-3645UV (LLDPE)
Want to keep this datasheet? Save it now in your required format

Description

GREENETHENE G-3645UV is a Low Density Linear Polyethylene Resin (LLDPE) in powder form, additivated with antioxidants and UV stabilizers. It is suitable for Rotational Molding applications. Items produced by GREENETHENE G-3645UV have a very good balance between mechanical properties and ESCR resistance. G-3645UV is produced in: natural, black, terracotta, fire red, yellow & blue. GREENETHENE G-3645UV meets the requirement stipulated in standard IS:10141:2001 on “Specification for Polyethylene for safe use in contact with foodstuff, pharmaceuticals & Drinking Water”. It also conforms to IS 12701:1996 –“Specification For Rotational Moulded Polyethylene Water Storage Tanks.”.

This material data has been provided by GreenAge Industries.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.94 g/cm³

Show Supplier Material materials with Density of 0.94 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

165 - 600 %

Show Supplier Material materials with Elongation of 165 - 600 %

ASTM D638

Flexural modulus

23.0 °C

0.23 - 0.59 GPa

Show Supplier Material materials with Flexural modulus of 0.23 - 0.59 GPa

ASTM D790

Hardness, Shore D

23.0 °C

55 [-]

Show Supplier Material materials with Hardness, Shore D of 55 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

250 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 250 J/m

ASTM D256

Tensile strength

23.0 °C

11.75 MPa

Show Supplier Material materials with Tensile strength of 11.75 MPa

ASTM D638

Yield strength

23.0 °C

17.5 - 18 MPa

Show Supplier Material materials with Yield strength of 17.5 - 18 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

117 °C

Show Supplier Material materials with Vicat softening temperature of 117 °C

ASTM D1525

Rheological Properties

PropertyValueComment

Melt mass-flow rate

4.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 4.5 g/10min

ASTM D1238, 190°C/2.16kg

Technological properties

Property
Application areas

Due to its combination of mechanical properties, ESCR resistance and fluidity, GREENETHENE G-3645UV is suggested for the production of wide variety of Storage tank applications of water, chemicals & Oils. GREENETHENE G-3645UV can also be used for off-shore flotation buoys and road crash barriers.

Certifications

List of Constituents of Polyethylene in Contact with Foodstuffs, Pharmaceuticals and Drinking Water: IS 10141:2001, IS 12701:1996

Color

Natural, black, terracotta, fire red, yellow and blue.

Processing methods

Compression molded & rotomolded