PA12 resins KH2070

Alternative and trade names
PEBAX 7033
Want to keep this datasheet? Save it now in your required format

Description

A long carbon chain PA12 elastomer

This material data has been provided by Global Star Trading (HK) Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.01 g/cm³

Show Supplier Material materials with Density of 1.01 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

0.4 GPa

Show Supplier Material materials with Flexural modulus of 0.4 GPa

ISO178

Hardness, Shore D

23.0 °C

69 - 70 [-]

Show Supplier Material materials with Hardness, Shore D of 69 - 70 [-]

ISO868

Impact strength, Charpy notched

-30.0 °C

20 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m²

ISO179, No break @23°C

Tensile strength

23.0 °C

54 MPa

Show Supplier Material materials with Tensile strength of 54 MPa

ISO527

Thermal

PropertyValueComment

Melting point

171 °C

Show Supplier Material materials with Melting point of 171 °C

ISO11357

Technological properties

Property
Application areas

Glass frames, eyeglasses frames, eyeglasses, sports sunglasses, watches, headphones, water cups, precipitation cups, filter cups, water-oil separators, fuel filter, filter filters, baby bottles, tea cups, edible oil bottles, cosmetics containers, dashboards, milk machinery shells, eyeglasses, water filter bowls, filter coverage, pneumatic air bowls.