PA12 resins TR128

Alternative and trade names
CX9704, G820
Want to keep this datasheet? Save it now in your required format

Description

Biological Matrix as Raw Material, Anti-chemcials & passed alcohol test, excellent transparency, high resilience and creep resistance, rigid and tough, excellent colouring and fuel injection adhesion

This material data has been provided by Global Star Trading (HK) Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.02 g/cm³

Show Supplier Material materials with Density of 1.02 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.6 GPa

Show Supplier Material materials with Elastic modulus of 1.6 GPa

ISO527

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

ISO527

Flexural modulus

23.0 °C

1.65 GPa

Show Supplier Material materials with Flexural modulus of 1.65 GPa

ISO178

Flexural strength

23.0 °C

58 MPa

Show Supplier Material materials with Flexural strength of 58 MPa

ISO178

Hardness, Ball Indentation

23.0 °C

90 MPa

Show Supplier Material materials with Hardness, Ball Indentation of 90 MPa

ISO2039-1

Hardness, Shore D

23.0 °C

82 [-]

Show Supplier Material materials with Hardness, Shore D of 82 [-]

ISO868

Impact strength, Charpy notched

-30.0 °C

14 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 14 kJ/m²

ISO179, No break @-30, 23°C

23.0 °C

11 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m²

ISO179, No break @-30, 23°C

Tensile strength

23.0 °C

61 MPa

Show Supplier Material materials with Tensile strength of 61 MPa

ISO527

Impact strength, Charpy unnotched

No break @-30, 23°C

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

122 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 122 °C

ISO 75/B

Heat deflection temperature, 1.80 MPa

108 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 108 °C

ISO75/A

Technological properties

Property
Application areas

Memory glasses frame, headphones, cosmetic; Electronic connector, infrared sensor cover, mobile, phone shell; Oil cup, clasp, handle, flowmeter, observing Mirror/Window, Oil nozzle cover, milker; Sanitary ware: bracket, water pipe/pressure regulating valve, water filter, window, flowmeter; Food containers: drinking cups, transparent containers, transparent tableware; Motion device: diving device shield, knife handle, waterproof watch case; Medical devices: Protective mask mirror, hearing aid/earphone/ear hang, respiratory mask

Processing methods

Drying Temperature: 90-100°C, Drying Time: 6-7 hr, Rear Temperature: 200°C, Middle Temperature: 240°C, Front Temperature: 250°C, Nozzle Temperature: 230°C, Mold Temperature: 70-100°C, Injection Pressure: 70-100 MPa