PA12 resins K3G20

Alternative and trade names
EMS LV2H LV-3H LV-4H LV-5H
Want to keep this datasheet? Save it now in your required format

Description

Oil resistance, low water absorption and size stability

This material data has been provided by Global Star Trading (HK) Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.17 g/cm³

Show Supplier Material materials with Density of 1.17 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

4.5 GPa

Show Supplier Material materials with Elastic modulus of 4.5 GPa

ISO527

Elongation

23.0 °C

10 %

Show Supplier Material materials with Elongation of 10 %

ISO527

Hardness, Shore D

23.0 °C

73 [-]

Show Supplier Material materials with Hardness, Shore D of 73 [-]

ISO868

Impact strength, Charpy notched

-30.0 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m²

ISO179

23.0 °C

20 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m²

ISO179

Impact strength, Charpy unnotched

-30.0 °C

68 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 68 kJ/m²

ISO179

23.0 °C

70 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 70 kJ/m²

ISO179

Unlock all property charts

Tensile strength

23.0 °C

90 MPa

Show Supplier Material materials with Tensile strength of 90 MPa

ISO527

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

150 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 150 °C

ISO75/A

Technological properties

Property
Application areas

Tubing connection; Automotive lightweight components; Sport health equipment

Fillers

20% Glass Fiber

Processing methods

Drying Temperature: 80-85°C, Drying Time: 3-4 hr, Rear Temperature: 190°C, Middle Temperature: 210°C, Front Temperature: 220°C, Nozzle Temperature: 210°C, Mold Temperature: 40-60°C, Injection Pressure: 80-100 MPa