PA12 resins KH3030I

Alternative and trade names
EMS L425W40 L25W40X
Want to keep this datasheet? Save it now in your required format

Description

Oil resistance, pipe grade, excellent low temp of flexibility

This material data has been provided by Global Star Trading (HK) Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.02 g/cm³

Show Supplier Material materials with Density of 1.02 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.5 GPa

Show Supplier Material materials with Elastic modulus of 0.5 GPa

ISO527

Elongation

23.0 °C

100 %

Show Supplier Material materials with Elongation of 100 %

ISO527

Hardness, Shore D

23.0 °C

62 [-]

Show Supplier Material materials with Hardness, Shore D of 62 [-]

ISO868

Impact strength, Charpy notched

-30.0 °C

13 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m²

ISO179, No break @-30°C

Tensile strength

23.0 °C

40 MPa

Show Supplier Material materials with Tensile strength of 40 MPa

ISO527

Yield strength

23.0 °C

26 MPa

Show Supplier Material materials with Yield strength of 26 MPa

ISO527

Impact strength, Charpy unnotched

No break @-30, 23°C

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

96 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 96 °C

ISO 75/B

Heat deflection temperature, 1.80 MPa

48 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 48 °C

ISO75/A

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC60112

Dielectric strength

23.0 °C

32 kV/mm

Show Supplier Material materials with Dielectric strength of 32 kV/mm

IEC60243-1

Volume resistivity

23.0 °C

1.00E+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm

IEC60093

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.9 - 1.3 %

Show Supplier Material materials with Shrinkage of 0.9 - 1.3 %

Technological properties

Property
Application areas

Oil tube, corrugated tube

Processing methods

Drying Temperature: 80-85°C, Drying Time: 4-6 hr, Rear Temperature: 200°C, Middle Temperature: 210°C, Front Temperature: 220°C, Nozzle Temperature: 230°C