PA610 resins K0095

Alternative and trade names
Dupont RS 3061HSL RS3261TL
Want to keep this datasheet? Save it now in your required format

Description

Low water absorption, excellent low temperature performace, self-lubrication and wear resistance, excellent resilience, oil resistance

This material data has been provided by Global Star Trading (HK) Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.08 g/cm³

Show Supplier Material materials with Density of 1.08 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.4 GPa

Show Supplier Material materials with Elastic modulus of 2.4 GPa

ISO527

Elongation

23.0 °C

200 %

Show Supplier Material materials with Elongation of 200 %

ISO527

Impact strength, Charpy notched

-30.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

ISO179

23.0 °C

9 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO179

Tensile strength

23.0 °C

60 MPa

Show Supplier Material materials with Tensile strength of 60 MPa

ISO527

Thermal

PropertyValueComment

Glass transition temperature

60 °C

Show Supplier Material materials with Glass transition temperature of 60 °C

ISO11357-1

Heat deflection temperature, 1.80 MPa

65 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 65 °C

ISO75/A

Melting point

215 °C

Show Supplier Material materials with Melting point of 215 °C

ISO11357-1

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

1.3 - 1.4 %

Show Supplier Material materials with Shrinkage of 1.3 - 1.4 %

Technological properties

Property
Application areas

Gears, battery cover, toothbrush wire, industrial brush wire

Processing methods

Drying Temperature: 80-85°C, Drying Time: 4-5 hr, Rear Temperature: 215°C, Middle Temperature: 220°C, Front Temperature: 225°C, Nozzle Temperature: 225°C, Mold Temperature: 40-60°C, Injection Pressure: 80-100 MPa