Description

Excellent resilience, self-lubrication and wear resistance, low water absorption, oil resistance, excellent low temperature performance

This material data has been provided by Global Star Trading (HK) Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.07 g/cm³

Show Supplier Material materials with Density of 1.07 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.4 GPa

Show Supplier Material materials with Elastic modulus of 2.4 GPa

ISO527

Elongation

23.0 °C

300 %

Show Supplier Material materials with Elongation of 300 %

ISO527

Impact strength, Charpy notched

-30.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

ISO179

23.0 °C

9 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO179

Tensile strength

23.0 °C

68 MPa

Show Supplier Material materials with Tensile strength of 68 MPa

ISO527

Thermal

PropertyValueComment

Glass transition temperature

60 °C

Show Supplier Material materials with Glass transition temperature of 60 °C

ISO11357-1

Heat deflection temperature, 1.80 MPa

68 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 68 °C

ISO75/A

Melting point

210 °C

Show Supplier Material materials with Melting point of 210 °C

ISO11357-1

Technological properties

Property
Application areas

Toothbrush wire, industrial brush wire, battery end cap, Gears

Processing methods

Drying Temperature: 80-85°C, Drying Time: 4-5 hr, Rear Temperature: 215°C, Middle Temperature: 220°C, Front Temperature: 225°C, Nozzle Temperature: 225°C, Mold Temperature: 60-80°C, Injection Pressure: 80-100 MPa