Styrene Butadiene Rubber (SBR) (30 mesh rubber) with 40-55% polymer content and 10-20% acetone expandable.

This material data has been provided by Heffco Elastomers Inc..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Moisture absorption

1 %

Show Supplier Material materials with Moisture absorption of 1 %

max.

Relative density

1.0 - 1.4 [-]

Show Supplier Material materials with Relative density of 1.0 - 1.4 [-]

Thermal

PropertyValue

Ash content

1.8 %

Show Supplier Material materials with Ash content of 1.8 %

Technological properties

Property
Particle size range table

100% passing 30 mesh