Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Styrene Butadiene Rubber (SBR) Heffco 230P
Styrene Butadiene Rubber (SBR) (30 mesh crumb rubber) powder with 27% polymer content and 18% acetone expandable.
This material data has been provided by Heffco Elastomers Inc..
All categories
Rubber & Plastic Industries
Rubber & Plastics Products
Piping Components
Hoses
Electrical Engineering
Electrical Insulation
Other Insulating Materials
Automotive
General Automotive Parts
Braking System
Tires
Road Vehicle Systems
Braking Systems
Aerospace
Aerospace Materials
Rubber & Plastics
Raw Materials For Rubber & Plastics
Rubber & Plastics Products In General
Polymeric Seals
Other Rubber & Plastics Products
Construction
Construction Materials
Binders.Sealing Materials
Thermal & Sound Insulating Materials
Buildings Protection
Acoustics In Building
Civil Engineering
Road Engineering
Road Construction Materials
Consumer Goods
Sports Equipment & Facilities
Sports Facilities
General
Property | Value | Comment |
---|---|---|
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | max. |
Relative density | 1.3 - 1.5 [-] Show Supplier Material materials with Relative density of 1.3 - 1.5 [-] |
Thermal
Property | Value |
---|---|
Ash content | 55.0 % Show Supplier Material materials with Ash content of 55.0 % |
Technological properties
Property | ||
---|---|---|
Particle size range table | 100% passing 30 mesh |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2022 Matmatch GmbH, All rights reserved.
Made with ❤️ in Munich!