Description

The stainless austenitic special steel 1.4462 has good resistance to pitting. Depending on the requirements and conditions, it is used in chemical equipment, pulp and food industries as well as for sea water piping systems.

Equivalent Materials

This material data has been provided by Hempel Special Metals.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7 g/cm³

Show Supplier Material materials with Density of 7 g/cm³

Mechanical

PropertyTemperatureValueComment

Hardness, Brinell

23.0 °C

270 [-]

Show Supplier Material materials with Hardness, Brinell of 270 [-]

max.

Chemical properties

PropertyValueComment

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

max.

Chromium

21 - 23 %

Show Supplier Material materials with Chromium of 21 - 23 %

Copper

0.11 %

Show Supplier Material materials with Copper of 0.11 %

max.

Iron

Balance

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

max.

Nickel

2.5 - 3.5 %

Show Supplier Material materials with Nickel of 2.5 - 3.5 %

Nitrogen

0.1 - 0.22 %

Show Supplier Material materials with Nitrogen of 0.1 - 0.22 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

max.

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

1.4462 is used mainly in sector of chemical industry, petrochemical industry, offshore, sea water lines, sea water desalination plants, nuclear engineering, paper and pulp industry.