Titanium 6-6-2 is a heat treatable high strength titanium alloy with lower toughness and ductility than Titanium 6Al/4V. Titanium 6-6-2 has a similar machinability to Austenitic steel , easily welded providing precautions are taken to shield against Oxygen, Hydrogen and Nitrogen contaminants