Description

Alloy 201 has excellent resistance to many corrosive media from acid to alkaline and is corrosion resistant. Alloy 201 offers good mechanical properties within a wide range of temperatures as well as magnetic and magnetostrictive properties and useful thermal and electrical conductivities.

Related Standards

Equivalent Materials

This material data has been provided by Hempel Special Metals.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Supplier Material materials with Density of 8.9 g/cm³

Thermal

PropertyValue

Melting point

1435 - 1445 °C

Show Supplier Material materials with Melting point of 1435 - 1445 °C

Chemical properties

PropertyValue

Carbon

0.02 %

Show Supplier Material materials with Carbon of 0.02 %

Copper

0.25 %

Show Supplier Material materials with Copper of 0.25 %

Iron

0.04 %

Show Supplier Material materials with Iron of 0.04 %

Magnesium

0.15 %

Show Supplier Material materials with Magnesium of 0.15 %

Manganese

0.35 %

Show Supplier Material materials with Manganese of 0.35 %

Nickel

90 %

Show Supplier Material materials with Nickel of 90 %

Silicon

0.2 %

Show Supplier Material materials with Silicon of 0.2 %

Sulfur

0.01 %

Show Supplier Material materials with Sulfur of 0.01 %

Titanium

0.1 %

Show Supplier Material materials with Titanium of 0.1 %

Technological properties

Property
Application areas

Alloy 201 is commonly used in food industry, but it is also in used vessels up to 600°C and sodium hydroxide evaporators up to 450°C. Alloy 201 is also often used in vessels for production of flour, hydrochloric acid or vinylchloride monomer.

Welding

Filler metal (for welding with 2.4066/2.4068)

  • 2.4155, 2.4620, 2.4806,
  • covered electrodes 2.4156