Titanium is preferred in medical industry due to its favourable biomedical properties - inertness and corrosion resistance to body fluids and tissue, high strength-to-weight ratio.

Related Standards

Equivalent Materials

This material data has been provided by Hempel Special Metals.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

4.43 g/cm³

Show Supplier Material materials with Density of 4.43 g/cm³

Mechanical

PropertyTemperatureValueComment

Elongation A50

23.0 °C

10 %

Show Supplier Material materials with Elongation A50 of 10 %

min.

Tensile strength

23.0 °C

860 MPa

Show Supplier Material materials with Tensile strength of 860 MPa

Yield strength Rp0.2

23.0 °C

780 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 780 MPa

Chemical properties

PropertyValueComment

Aluminium

5.5 - 6.5 %

Show Supplier Material materials with Aluminium of 5.5 - 6.5 %

Carbon

0.08 %

Show Supplier Material materials with Carbon of 0.08 %

max.

Hydrogen

0.01 %

Show Supplier Material materials with Hydrogen of 0.01 %

max.

Iron

0.25 %

Show Supplier Material materials with Iron of 0.25 %

max.

Nitrogen

0.05 %

Show Supplier Material materials with Nitrogen of 0.05 %

max.

Titanium

Balance

Vanadium

3.5 - 4.5 %

Show Supplier Material materials with Vanadium of 3.5 - 4.5 %

Technological properties

Property
Application areas

Titanium Grade 23 ELI is found as most used alloy in medical industry for shoulder implants, hip-balls osteosyntheses, bone screws, bone plates, marrow-nails, spinalsystems, dental implants and tools. It's used also for:


  • Watch cases
  • Jewellery elements
  • Aerospace industry