PP TOPILENE® R200P-3702

Alternative and trade names
TOPILENE® R200P-3702
Want to keep this datasheet? Save it now in your required format

Description

Polypropylene random copolymer for PPR pipe is a high molecular weight polymer with high melt viscosity. Because of this characteristic, it is not easy to mix natural resin with color master batch during pipe production. Therefore, we recommend using pre-colored R200P for better quality. Through excellent compounding technology and In-line coloring process, Hyosung Chemical supplies world best reliable quality pre-colored PPR Topilene® R200P.

This material data has been provided by Hyosung Chemical Corporation.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 g/cm³

Show Supplier Material materials with Density of 0.9 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

0.88 GPa

Show Supplier Material materials with Flexural modulus of 0.88 GPa

ASTM D790

Hardness, Rockwell R

23.0 °C

75 [-]

Show Supplier Material materials with Hardness, Rockwell R of 75 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

-10.0 °C

50 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 50 J/m

ASTM D256

Yield strength

23.0 °C

26.48 MPa

Show Supplier Material materials with Yield strength of 26.48 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

80.0 °C

1.5E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-4 1/K

Mean value between 0°C and the mentioned temperature, Dilatometer

Heat deflection temperature, 0.45 MPa

90 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 90 °C

ASTM D648

Melting point

141 °C

Show Supplier Material materials with Melting point of 141 °C

ASTM D3418

Vicat softening temperature

130 °C

Show Supplier Material materials with Vicat softening temperature of 130 °C

ASTM D1525

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

1.00E+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq

Minimum, ASTM HS Method

Rheological Properties

PropertyValueComment

Melt mass-flow rate

0.25 g/10min

Show Supplier Material materials with Melt mass-flow rate of 0.25 g/10min

ASTM D1238

Technological properties

Property
Application areas

Pipes and fittings, piping for house, radiator pipes, idustrial pipes