PP TOPILENE® R200P-G40N

Alternative and trade names
TOPILENE® R200P-G40N
Want to keep this datasheet? Save it now in your required format

Description

As a substitute for Aluminum-PPR composite pipe, GF(Glass Fiber)-PPR composite pipe has been widely used for hot & cold water supply system. Topilene® R200P GF has an excellent binding strength between glass fiber and PPR, providing outstanding hydrostatic pressure resistance level. Based on technical know-how we have accumulated for decades, Topilene® R200P GF composite is manufactured with well-controlled glass fiber, offering an excellent pipe surface and physical properties.

This material data has been provided by Hyosung Chemical Corporation.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.21 g/cm³

Show Supplier Material materials with Density of 1.21 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

3.92 GPa

Show Supplier Material materials with Flexural modulus of 3.92 GPa

ASTM D790

Hardness, Rockwell R

23.0 °C

90 [-]

Show Supplier Material materials with Hardness, Rockwell R of 90 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

-10.0 °C

50 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 50 J/m

ASTM D256

23.0 °C

140 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 140 J/m

ASTM D256

Yield strength

23.0 °C

51.98 MPa

Show Supplier Material materials with Yield strength of 51.98 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

135 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C

ASTM D648

Melting point

146 °C

Show Supplier Material materials with Melting point of 146 °C

ASTM D3418

Vicat softening temperature

145 °C

Show Supplier Material materials with Vicat softening temperature of 145 °C

ASTM D1525

Rheological Properties

PropertyValueComment

Melt mass-flow rate

0.3 g/10min

Show Supplier Material materials with Melt mass-flow rate of 0.3 g/10min

ASTM D1238

Technological properties

Property
Application areas

Pipes and fittings, piping for house, radiator pipes, idustrial pipes

Fillers

40% Glass Fiber