PP TOPILENE® HB242P

Alternative and trade names
TOPILENE® HB242P
Want to keep this datasheet? Save it now in your required format

Description

TOPILENE® HB242P is a High Modulus PP impact copolymer (PP-HM). It shows very high stiffness and an excellent impact strength providing superior processing characteristics. HB242P makes it possible to produce thinner wall PP pipe while keeping the same ring stiffness of normal PP-B pipes.

This material data has been provided by Hyosung Chemical Corporation.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 g/cm³

Show Supplier Material materials with Density of 0.9 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.77 GPa

Show Supplier Material materials with Flexural modulus of 1.77 GPa

ASTM D790

Hardness, Rockwell R

23.0 °C

95 [-]

Show Supplier Material materials with Hardness, Rockwell R of 95 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

-10.0 °C

50 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 50 J/m

ASTM D256

Yield strength

23.0 °C

31.38 MPa

Show Supplier Material materials with Yield strength of 31.38 MPa

ASTM D638

Thermal

PropertyValueComment

Melting point

167 °C

Show Supplier Material materials with Melting point of 167 °C

ASTM D3418

Rheological Properties

PropertyValueComment

Melt mass-flow rate

0.3 g/10min

Show Supplier Material materials with Melt mass-flow rate of 0.3 g/10min

ASTM D1238

Technological properties

Property
Application areas

Sewer/drainage pipes (solid wall type-corrugated type), storm water drainage system