Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Find Materials
Categories
Butadiene Rubber (BR) GND45
Linear BR(Butadiene Rubber) is a synthetic rubber made by applying solution polymerization method on butadiene. It has a higher proportion of cis isomers (96% content). BR is used largely for tires, shoes and golf balls because of its excellent wear resistance, bend resistance, rebound resilience and cold resistance.
This material data has been provided by LG Chem.
All categories
Rheological Properties
Property | Value |
---|---|
Mooney viscosity | 45 MU Show Supplier Material materials with Mooney viscosity of 45 MU |
Technological properties
Property | ||
---|---|---|
Application areas | High Resilience, Wear resistance, Cold resistance (Tire, Shoe-sole, Golf ball, Belt) | |
Other | It should be stored in warehouse to be protected from sunlight, heat and moisture. Shelf life : 24 months from date of production at room temperature not exceeding 30°C under above storage condition. (Retest critical parameters like MV and others after the expiry of shelf life) | |
Processing history | Catalyst: neodymium |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.