General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 1.05 g/cm³ Show Supplier Material materials with Density of 1.05 g/cm³ at 23.0 °C | 23.0 °C | ASTM D297 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 500 % Show Supplier Material materials with Elongation of 500 % at 23.0 °C | 23.0 °C | ASTM D412 |
Hardness, Shore A | 60 [-] Show Supplier Material materials with Hardness, Shore A of 60 [-] at 23.0 °C | 23.0 °C | |
Tensile strength | 6.5 MPa Show Supplier Material materials with Tensile strength of 6.5 MPa at 23.0 °C | 23.0 °C | ASTM D412 |
Thermal
Property | Value |
---|---|
Flammability | HB |
Electrical
Property | Value | Temperature | Comment |
---|---|---|---|
Dielectric constant, 1MHz | 2.3 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.3 [-] at 23.0 °C | 23.0 °C | ASTM D150 |
Dielectric strength | 28 kV/mm Show Supplier Material materials with Dielectric strength of 28 kV/mm at 23.0 °C | 23.0 °C | ASTM D149 |
Dissipation factor, 1MHz | 4E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-] at 23.0 °C | 23.0 °C | ASTM D150 |
Volume resistivity | 1.00E+19 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+19 Ω·cm at 23.0 °C | 23.0 °C | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive interior | |
Fillers | 25% Calcium Carbonate | |
Processing methods | Injection Molding, Extrusion |