TPV 60A

This material data has been provided by Lingen Plastic Rubber Co..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperatureComment

Density

0.96 g/cm³

Show Supplier Material materials with Density of 0.96 g/cm³ at 23.0 °C

23.0 °C

ASTM D297

Mechanical

PropertyValueTemperatureComment

Elongation

400 %

Show Supplier Material materials with Elongation of 400 % at 23.0 °C

23.0 °C

ASTM D412

Hardness, Shore A

60 [-]

Show Supplier Material materials with Hardness, Shore A of 60 [-] at 23.0 °C

23.0 °C

Tensile strength

4.2 MPa

Show Supplier Material materials with Tensile strength of 4.2 MPa at 23.0 °C

23.0 °C

ASTM D412

Thermal

PropertyValue

Flammability

HB

Electrical

PropertyValueTemperatureComment

Dielectric constant, 1MHz

2.3 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.3 [-] at 23.0 °C

23.0 °C

ASTM D150

Dielectric strength

28 kV/mm

Show Supplier Material materials with Dielectric strength of 28 kV/mm at 23.0 °C

23.0 °C

ASTM D149

Dissipation factor, 1MHz

4E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-] at 23.0 °C

23.0 °C

ASTM D150

Volume resistivity

1.00E+19 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+19 Ω·cm at 23.0 °C

23.0 °C

min., ASTM D257

Technological properties

Property
Application areas

Automotive exterior

Fillers

10% Talc

Processing methods

Injection Molding, Extrusion