Description

Thermalox® 995 ceramic - offers the second highest thermal conductivity of all our BeO ceramics.

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.85 g/cm³

Show Supplier Material materials with Density of 2.85 g/cm³

Grain size

15 μm

Show Supplier Material materials with Grain size of 15 μm

Water absorption

23.0 °C

0 %

Show Supplier Material materials with Water absorption of 0 %

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

1.55 MPa

Show Supplier Material materials with Compressive strength of 1.55 MPa

Elastic modulus

23.0 °C

345 GPa

Show Supplier Material materials with Elastic modulus of 345 GPa

Flexural strength

23.0 °C

221 MPa

Show Supplier Material materials with Flexural strength of 221 MPa

Hardness, Rockwell Superficial 45-N

23.0 °C

60 [-]

Show Supplier Material materials with Hardness, Rockwell Superficial 45-N of 60 [-]

Plane-Strain Fracture Toughnes

23.0 °C

3.5 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.5 MPa·√m

Poisson's ratio

23.0 °C

0.26 [-]

Show Supplier Material materials with Poisson's ratio of 0.26 [-]

Tensile strength

23.0 °C

152 MPa

Show Supplier Material materials with Tensile strength of 152 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

9E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9E-6 1/K

Specific heat capacity

23.0 °C

1046 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 1046 J/(kg·K)

Thermal conductivity

23.0 °C

285 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 285 W/(m·K)

Electrical

PropertyTemperatureValueComment

Dielectric constant, 10GHz

23.0 °C

6.76 [-]

Show Supplier Material materials with Dielectric constant, 10GHz of 6.76 [-]

Dielectric constant, 1MHz

23.0 °C

6.76 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 6.76 [-]

Dielectric strength

23.0 °C

0.23 kV/mm

Show Supplier Material materials with Dielectric strength of 0.23 kV/mm

AC, 6.35mm

Dissipation factor, 1MHz

23.0 °C

4E-4 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-4 [-]

Electrical resistivity

23.0 °C

1.00E+13 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+13 Ω·m

Minimum

Technological properties

Property
Application areas

Medical, industrial and electronics markets, dosimeters, crucibles for Li-ion batteries, aerospace applications for thermal management, medical imaging applications, defense systems and electronics manufacturing

Color

White