BW 1000

Want to keep this datasheet? Save it now in your required format

Description

BW 1000® is 99.5% pure BeO and delivers improved performance for circuits and applications generating high heat. BeO has a lower dielectric constant of 6.7 compared to AlN's 9.7 dielectric constant. BW ceramics offer electrical resistivity and dielectric strength equivalent to competitive materials.


BW 1000 ceramic offers the highest flexural strength (MOR) of all our beryilla grades. When small components require great strength, BW 1000 ceramic is the optimum choice. This ceramic material is ideal for very small, fragile parts that will endure high levels of stress during the life cycle of the product.

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.89 g/cm³

Show Supplier Material materials with Density of 2.89 g/cm³

Grain size

14 μm

Show Supplier Material materials with Grain size of 14 μm

Water absorption

23.0 °C

0 %

Show Supplier Material materials with Water absorption of 0 %

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

1.55 MPa

Show Supplier Material materials with Compressive strength of 1.55 MPa

Elastic modulus

23.0 °C

345 GPa

Show Supplier Material materials with Elastic modulus of 345 GPa

Flexural strength

23.0 °C

262 MPa

Show Supplier Material materials with Flexural strength of 262 MPa

Hardness, Rockwell Superficial 45-N

23.0 °C

60 [-]

Show Supplier Material materials with Hardness, Rockwell Superficial 45-N of 60 [-]

Plane-Strain Fracture Toughnes

23.0 °C

3.7 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.7 MPa·√m

Poisson's ratio

23.0 °C

0.26 [-]

Show Supplier Material materials with Poisson's ratio of 0.26 [-]

Tensile strength

23.0 °C

172 MPa

Show Supplier Material materials with Tensile strength of 172 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

9E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9E-6 1/K

Specific heat capacity

23.0 °C

1046 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 1046 J/(kg·K)

Thermal conductivity

23.0 °C

275 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 275 W/(m·K)

Electrical

PropertyTemperatureValueComment

Dielectric constant, 10GHz

23.0 °C

6.76 [-]

Show Supplier Material materials with Dielectric constant, 10GHz of 6.76 [-]

Dielectric constant, 1MHz

23.0 °C

6.76 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 6.76 [-]

Dielectric strength

23.0 °C

0.23 kV/mm

Show Supplier Material materials with Dielectric strength of 0.23 kV/mm

AC, 6.35mm

Dissipation factor, 1MHz

23.0 °C

4E-4 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-4 [-]

Electrical resistivity

23.0 °C

1.00E+13 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+13 Ω·m

Minimum

Technological properties

Property
Application areas

Medical equipment, military applications, electronic components and traveling wave tubes (TWT)

Color

White