Durox 98

Want to keep this datasheet? Save it now in your required format

Description

This alumina oxide ceramic is 97.6% pure Al2O3 and is the most affordable alumina ceramic option for ceramic components.

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

3.83 g/cm³

Show Supplier Material materials with Density of 3.83 g/cm³

Grain size

2 μm

Show Supplier Material materials with Grain size of 2 μm

Water absorption

23.0 °C

0 %

Show Supplier Material materials with Water absorption of 0 %

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

2.41 MPa

Show Supplier Material materials with Compressive strength of 2.41 MPa

Elastic modulus

23.0 °C

351 GPa

Show Supplier Material materials with Elastic modulus of 351 GPa

Flexural strength

23.0 °C

379 MPa

Show Supplier Material materials with Flexural strength of 379 MPa

Hardness, Rockwell Superficial 45-N

23.0 °C

85 [-]

Show Supplier Material materials with Hardness, Rockwell Superficial 45-N of 85 [-]

Plane-Strain Fracture Toughnes

23.0 °C

4 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 MPa·√m

Poisson's ratio

23.0 °C

0.22 [-]

Show Supplier Material materials with Poisson's ratio of 0.22 [-]

Tensile strength

23.0 °C

152 MPa

Show Supplier Material materials with Tensile strength of 152 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

7.5E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7.5E-6 1/K

RT to 1000°C

Specific heat capacity

23.0 °C

837.36 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 837.36 J/(kg·K)

Thermal conductivity

23.0 °C

27 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 27 W/(m·K)

Electrical

PropertyTemperatureValueComment

Dielectric constant, 10GHz

23.0 °C

9.4 [-]

Show Supplier Material materials with Dielectric constant, 10GHz of 9.4 [-]

Dielectric constant, 1MHz

23.0 °C

9.5 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 9.5 [-]

Dielectric strength

23.0 °C

0.22 kV/mm

Show Supplier Material materials with Dielectric strength of 0.22 kV/mm

AC, 6.35mm

Dissipation factor, 1MHz

23.0 °C

1E-4 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 1E-4 [-]

Electrical resistivity

23.0 °C

1.00E+13 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+13 Ω·m

Minimum

Technological properties

Property
Application areas

photonics/ lasers, defense, energy, telecommunications and semiconductor manufacturing

Color

Off White