SupremEX® 225XE T6PGQ Extruded Bar (AA2124)

Alternative and trade names
SupremEX® 225XE
Want to keep this datasheet? Save it now in your required format

Description

A high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% 3-micron silicon carbide which is manufactured via a powder metallurgy route using a high energy mixing process to ensure a homogeneous distribution of the reinforcement and to refine the grain structure to enhance mechanical properties. The alloy is heat treatable offering high strength and modulus for structural applications and is available in billet, forged and extruded forms.


225XE Advantages:


  • Weight saving
  • High Strength
  • Increased component stiffness
  • High fatigue resistance
  • Hardness, wear resistance & low friction characteristics
  • Good machinability using conventional techniques
  • Homogenous stable microstructure
  • Equivalent Materials

    This material data has been provided by Materion Brush GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    2.88 g/cm³

    Show Supplier Material materials with Density of 2.88 g/cm³

    Mechanical

    PropertyTemperatureValue

    Elastic modulus

    23.0 °C

    115 GPa

    Show Supplier Material materials with Elastic modulus of 115 GPa

    Elongation

    23.0 °C

    4 - 5 %

    Show Supplier Material materials with Elongation of 4 - 5 %

    Poisson's ratio

    23.0 °C

    0.3 [-]

    Show Supplier Material materials with Poisson's ratio of 0.3 [-]

    Tensile strength

    23.0 °C

    600 MPa

    Show Supplier Material materials with Tensile strength of 600 MPa

    Yield strength Rp0.2

    23.0 °C

    400 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 400 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    1.61E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.61E-5 1/K

    Melting point

    548 °C

    Show Supplier Material materials with Melting point of 548 °C

    Specific heat capacity

    23.0 °C

    848 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 848 J/(kg·K)

    Thermal conductivity

    23.0 °C

    150 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 150 W/(m·K)

    Technological properties

    Property
    Application areas

    Commercial and Military Aerospace: Outlet guide vanes, Hydraulic / Fuel blocks, Wheels, Fixed wing structure/ skins, Helicopter components - Commercial and Preformance Automotive: Pistons, Piston pins, Cylinder liners, Brake calipers, Connecting rods, Push rods, Valve train, Chassis components - Space, Defence and Optical Systems: Optical systems & sensors, Satellite structures, Astronomical telescopes

    Processing history

    Extrusion