Description

ToughMet Alloy is Materion Performance Alloys’ solution to your severe service material problems. By application of our proprietary process to implement the EquaCast® Microstructure, tailored alloying additions and spinodal hardening technology, we have engineered ToughMet alloy to provide attributes beyond those typically found in a high-strength copper alloy.


  • Exceptional resistance to corrosion and cavitation
  • Outstanding lubricity and durability in demanding applications
  • Highly uniform composition in all product forms
  • Uniform microstructure in a variety of wrought shapes and sizes
  • Related Standards

    This material data has been provided by Materion Brush GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueTemperature

    Density

    9 g/cm³

    Show Supplier Material materials with Density of 9 g/cm³ at 23.0 °C

    23.0 °C

    Dimension

    PropertyValue

    Thickness

    6.4 - 120.7 mm

    Show Supplier Material materials with Thickness of 6.4 - 120.7 mm

    Mechanical

    PropertyValueTemperatureComment

    Elastic modulus

    144 GPa

    Show Supplier Material materials with Elastic modulus of 144 GPa at 23.0 °C

    23.0 °C

    Elongation

    6 %

    Show Supplier Material materials with Elongation of 6 % at 23.0 °C

    23.0 °C

    Fatigue strength

    415 MPa

    Show Supplier Material materials with Fatigue strength of 415 MPa at 23.0 °C

    23.0 °C

    10⁶ cycles R=-1

    Hardness, Rockwell C

    30 [-]

    Show Supplier Material materials with Hardness, Rockwell C of 30 [-] at 23.0 °C

    23.0 °C

    Poisson's ratio

    0.33 [-]

    Show Supplier Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C

    23.0 °C

    Tensile strength

    860 MPa

    Show Supplier Material materials with Tensile strength of 860 MPa at 23.0 °C

    23.0 °C

    Yield strength Rp0.2

    760 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 760 MPa at 23.0 °C

    23.0 °C

    Thermal

    PropertyValueTemperature

    Coefficient of thermal expansion

    1.64E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.64E-5 1/K at 23.0 °C

    23.0 °C

    Thermal conductivity

    38 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 38 W/(m·K) at 23.0 °C

    23.0 °C

    Electrical

    PropertyValueTemperatureComment

    Electrical conductivity

    4.00E+6 S/m

    Show Supplier Material materials with Electrical conductivity of 4.00E+6 S/m at 23.0 °C

    23.0 °C

    max.

    Specific Electrical conductivity

    7 % IACS

    Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS

    max.

    Magnetic

    PropertyValueTemperature

    Relative magnetic permeability

    1 [-]

    Show Supplier Material materials with Relative magnetic permeability of 1 [-] at 23.0 °C

    23.0 °C

    Chemical properties

    Property

    Copper

    Balance

    Nickel

    15 %

    Tin

    8 %

    Technological properties

    Property
    Application areas

    ToughMet 3 AT alloy is used for bushings and bearings for commercial aircraft, high performance engines as well as mining, industrial and heavy equipment. It is also used to make oil and gas drilling hardware, including rotary steerable housings, kelly valve seats and pressure housings.