Description

ToughMet 3 TS alloy is a cold worked, spinodally hardened alloy designed to provide high strength for the most demanding static structural loads and pressures. It provides high toughness combined with high strength to resist dynamic impact loading. ToughMet 3 TS alloy provides galling resistance, high bearing performance and compatibility with many sour environments or salt water. It is non-magnetic and very easy to machine into complex components.

Related Standards

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

9 g/cm³

Show Supplier Material materials with Density of 9 g/cm³

Dimension

PropertyValue

Outside diameter

38 - 77 mm

Show Supplier Material materials with Outside diameter of 38 - 77 mm

Wall thickness

<10, >10

Mechanical

PropertyTemperatureValueComment

Charpy impact energy, V-notch

23.0 °C

14 - 19 J

Show Supplier Material materials with Charpy impact energy, V-notch of 14 - 19 J

Average value

Elastic modulus

23.0 °C

144 GPa

Show Supplier Material materials with Elastic modulus of 144 GPa

Elongation

23.0 °C

15 - 16 %

Show Supplier Material materials with Elongation of 15 - 16 %

in 4D

Hardness, Rockwell C

23.0 °C

22 [-]

Show Supplier Material materials with Hardness, Rockwell C of 22 [-]

Poisson's ratio

23.0 °C

0.33 [-]

Show Supplier Material materials with Poisson's ratio of 0.33 [-]

Tensile strength

23.0 °C

830 MPa

Show Supplier Material materials with Tensile strength of 830 MPa

Yield strength Rp0.2

23.0 °C

725 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 725 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.64E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.64E-5 1/K

Thermal conductivity

23.0 °C

38 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 38 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical conductivity

23.0 °C

4.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 4.00E+6 S/m

max.

Specific Electrical conductivity

7 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS

max.

Magnetic

PropertyTemperatureValue

Relative magnetic permeability

23.0 °C

1 [-]

Show Supplier Material materials with Relative magnetic permeability of 1 [-]

Technological properties

Property
Application areas

ToughMet 3 TS alloy tempers are commonly used in the oil and gas industry, oil & gas production via our sucker rod couplings and in commercial aircraft.