Description

ToughMet 3 Alloy is Materion Performance Alloys’ solution to your severe service material problems. By applying our proprietary technology process to create the EquaCast® microstructure, tailored alloying additions and spinodal hardening technology, we have engineered ToughMet 3 Alloy to provide attributes beyond those typically found in a high-strength copper alloy. ToughMet 3 Alloy in the cast and spinodally hardened (CX) condition exhibits tensile strength up to 120 ksi and hardness up to HRC 34 in a Copper - 15% Nickel - 8% Tin alloy with excellent machinability.


  • Exceptional resistance to corrosion and cavitation
  • Outstanding lubricity and durability in demanding applications
  • Highly uniform composition in all product forms
  • Available in a wide range of continuous-cast shapes and sizes
  • This material data has been provided by Materion Brush GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    9 g/cm³

    Show Supplier Material materials with Density of 9 g/cm³

    Dimension

    PropertyValue

    Inside diameter

    12.7 - 76.2 mm

    Show Supplier Material materials with Inside diameter of 12.7 - 76.2 mm

    Outside diameter

    28.6 - 254 mm

    Show Supplier Material materials with Outside diameter of 28.6 - 254 mm

    Wall thickness

    6.35 - 15.9 mm

    Show Supplier Material materials with Wall thickness of 6.35 - 15.9 mm

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    144 GPa

    Show Supplier Material materials with Elastic modulus of 144 GPa

    Elongation

    23.0 °C

    6 %

    Show Supplier Material materials with Elongation of 6 %

    Fatigue strength

    23.0 °C

    413 MPa

    Show Supplier Material materials with Fatigue strength of 413 MPa

    10⁶ cycles R=-1

    Hardness, Rockwell C

    23.0 °C

    27 [-]

    Show Supplier Material materials with Hardness, Rockwell C of 27 [-]

    Poisson's ratio

    23.0 °C

    0.3 [-]

    Show Supplier Material materials with Poisson's ratio of 0.3 [-]

    Tensile strength

    23.0 °C

    724 MPa

    Show Supplier Material materials with Tensile strength of 724 MPa

    Yield strength Rp0.2

    23.0 °C

    621 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 621 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    1.6E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

    Thermal conductivity

    23.0 °C

    38 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 38 W/(m·K)

    Electrical

    PropertyValue

    Specific Electrical conductivity

    9 % IACS

    Show Supplier Material materials with Specific Electrical conductivity of 9 % IACS

    Magnetic

    PropertyTemperatureValue

    Relative magnetic permeability

    23.0 °C

    1 [-]

    Show Supplier Material materials with Relative magnetic permeability of 1 [-]

    Chemical properties

    PropertyValue

    Copper

    Balance

    Nickel

    15 %

    Show Supplier Material materials with Nickel of 15 %

    Tin

    8 %

    Show Supplier Material materials with Tin of 8 %

    Technological properties

    Property
    Application areas

    ToughMet 3 CX alloy is used for wear plates, bushings, sleeve bearings, linear bearings and thrust bearings in industrial, off-road, mining and heavy equipment. It is also used for oil and gas drilling hardware.