AlBeCast 910® Composite

Alternative and trade names
AlBeCast 910®
Want to keep this datasheet? Save it now in your required format

Description

Materion's AlBeCast® product line is a family of investment cast aluminum-beryllium metal matrix composites that provides designers a net-shape product. Advantages over aluminium A356.0:

  • ~22% lower density
  • ~3 times stiffer (modulus of elasticity in tension)
  • Up to 10 times better in damping coefficient
  • ~40% lower in coefficient of thermal expansion (CTE)
  • ~50% higher specific heat
  • ~28% higher thermal conductivity

  • Advantages over beryllium:

  • ~3 times greater ductility than hot pressed beryllium with greater damage tolerance
  • Castable for complex and precise net shape configurations
  • Weldable for defect repair
  • Reduced machining and scrap generation
  • Reduced environmental processing concerns resulting from reduced waste
  • Does not require chemical etching
  • Reduced material usage
  • Reduced cost
  • This material data has been provided by Materion Brush GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    2.17 g/cm³

    Show Supplier Material materials with Density of 2.17 g/cm³

    Mechanical

    PropertyTemperatureValueComment

    Compressive yield strength

    23.0 °C

    147 MPa

    Show Supplier Material materials with Compressive yield strength of 147 MPa

    Elastic modulus

    23.0 °C

    193 GPa

    Show Supplier Material materials with Elastic modulus of 193 GPa

    Elongation

    23.0 °C

    4.7 %

    Show Supplier Material materials with Elongation of 4.7 %

    Fatigue strength

    23.0 °C

    86.2 MPa

    Show Supplier Material materials with Fatigue strength of 86.2 MPa

    10⁷ cycles, R=-1, Kt=1

    Poisson's ratio

    23.0 °C

    0.15 [-]

    Show Supplier Material materials with Poisson's ratio of 0.15 [-]

    Shear strength

    23.0 °C

    181 MPa

    Show Supplier Material materials with Shear strength of 181 MPa

    Pin Double Shear Strength

    Tensile strength

    23.0 °C

    196.5 MPa

    Show Supplier Material materials with Tensile strength of 196.5 MPa

    Yield strength Rp0.2

    23.0 °C

    147.5 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 147.5 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    1.46E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.46E-5 1/K

    Specific heat capacity

    23.0 °C

    1560 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 1560 J/(kg·K)

    Thermal conductivity

    23.0 °C

    110 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 110 W/(m·K)

    Electrical

    PropertyValue

    Specific Electrical conductivity

    48 % IACS

    Show Supplier Material materials with Specific Electrical conductivity of 48 % IACS

    Chemical properties

    PropertyValueComment

    Aluminium

    Balance

    Beryllium

    56 - 68 %

    Show Supplier Material materials with Beryllium of 56 - 68 %

    Cobalt

    0.2 %

    Show Supplier Material materials with Cobalt of 0.2 %

    max

    Germanium

    0.2 %

    Show Supplier Material materials with Germanium of 0.2 %

    max.

    Iron

    0.45 %

    Show Supplier Material materials with Iron of 0.45 %

    max.

    Nickel

    2.4 - 3.5 %

    Show Supplier Material materials with Nickel of 2.4 - 3.5 %

    Silicon

    0.2 %

    Show Supplier Material materials with Silicon of 0.2 %

    max.

    Silver

    0.2 %

    Show Supplier Material materials with Silver of 0.2 %

    max.

    Technological properties

    Property