BrushCAST® 3C as cast

Alternative and trade names
BrushCAST® 3C
Want to keep this datasheet? Save it now in your required format

Description

Alloy 3C offers excellent electrical and thermal conductivity, good strength & galling resistance, and accurate replication of component detail. Alloy 3C offers nearly 3 times the conductivity of the high strength alloys, twice the thermal conductivity of aluminum alloys, and ten times that of steel.

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.83 g/cm³

Show Supplier Material materials with Density of 8.83 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

140 GPa

Show Supplier Material materials with Elastic modulus of 140 GPa

Elongation

23.0 °C

15 - 25 %

Show Supplier Material materials with Elongation of 15 - 25 %

Hardness, Rockwell B

23.0 °C

55 - 65 [-]

Show Supplier Material materials with Hardness, Rockwell B of 55 - 65 [-]

Tensile strength

23.0 °C

380 - 410 MPa

Show Supplier Material materials with Tensile strength of 380 - 410 MPa

Yield strength Rp0.2

23.0 °C

170 - 240 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 170 - 240 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Thermal conductivity

23.0 °C

250 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 250 W/(m·K)

Electrical

PropertyValue

Specific Electrical conductivity

45 - 50 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 45 - 50 % IACS

Technological properties

Property
Application areas

For plastic mold making, die cast plunger tips, non-sparking safety tools, parts for defense applications and undersea components.