Description

BrushCAST high strength casting alloys provide peak strength and hardness greater than many steels, but with thermal conductivity similar to that of aluminum and up to five times that of steel. Additionally these alloys offer good electrical conductivity, excellent wear and galling resistance, and the highest accuracy in replicating fine detail in cast components

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.3 g/cm³

Show Supplier Material materials with Density of 8.3 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

130 GPa

Show Supplier Material materials with Elastic modulus of 130 GPa

Elongation

23.0 °C

10 - 20 %

Show Supplier Material materials with Elongation of 10 - 20 %

Hardness, Rockwell C

23.0 °C

20 - 24 [-]

Show Supplier Material materials with Hardness, Rockwell C of 20 - 24 [-]

Tensile strength

23.0 °C

690 - 720 MPa

Show Supplier Material materials with Tensile strength of 690 - 720 MPa

Yield strength Rp0.2

23.0 °C

480 - 520 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 480 - 520 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Thermal conductivity

23.0 °C

56 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 56 W/(m·K)

Electrical

PropertyValue

Specific Electrical conductivity

18 - 25 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 18 - 25 % IACS

Technological properties

Property
Application areas

For plastic mold making, die cast plunger tips, non-sparking safety tools, parts for defense applications and undersea components.