Alloy 25 Strip TD01 (C17200)

Alternative and trade names
Alloy 25 (C17200) Strip
Want to keep this datasheet? Save it now in your required format

Description

Materion Brush Performance Alloys’ Alloy 25 strip provides the highest strength of any copper alloy, with electrical conductivity considerably greater than other high strength copper alloys. Since it is heat treated after forming, it provides excellent formability and ductility. This alloy features good stress relaxation resistance and high fatigue strength.

Related Standards

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.36 g/cm³

Show Supplier Material materials with Density of 8.36 g/cm³

Dimension

PropertyValue

Thickness

0.05 - 4.77 mm

Show Supplier Material materials with Thickness of 0.05 - 4.77 mm

Width

1.27 - 406.5 mm

Show Supplier Material materials with Width of 1.27 - 406.5 mm

Mechanical

PropertyTemperatureValueComment

Bendability 90°, bw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 90°, bw of 0 [-]

for strip with 0.25mm and thinner.

Bendability 90°, gw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 90°, gw of 0 [-]

for strip with 0.25mm and thinner.

Elastic modulus

23.0 °C

131 GPa

Show Supplier Material materials with Elastic modulus of 131 GPa

Elongation

23.0 °C

20 - 45 %

Show Supplier Material materials with Elongation of 20 - 45 %

Hardness, Vickers

23.0 °C

121 - 185 [-]

Show Supplier Material materials with Hardness, Vickers of 121 - 185 [-]

Tensile strength

23.0 °C

510 - 610 MPa

Show Supplier Material materials with Tensile strength of 510 - 610 MPa

Yield strength Rp0.2

23.0 °C

410 - 560 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 410 - 560 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.75E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

Melting point

870 °C

Show Supplier Material materials with Melting point of 870 °C

Thermal conductivity

23.0 °C

105 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 105 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

6.2E-6 - 7.8E-6 Ω·m

Show Supplier Material materials with Electrical resistivity of 6.2E-6 - 7.8E-6 Ω·m

Specific Electrical conductivity

22 - 28 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 22 - 28 % IACS

Chemical properties

PropertyValueComment

Beryllium

1.8 - 2 %

Show Supplier Material materials with Beryllium of 1.8 - 2 %

Cobalt

0.2 %

Show Supplier Material materials with Cobalt of 0.2 %

min. Nickel + Cobalt

Copper

Balance

Iron

0.6 %

Show Supplier Material materials with Iron of 0.6 %

max., Nickel + Cobalt + Iron

Nickel

0.2 %

Show Supplier Material materials with Nickel of 0.2 %

min. Nickel + Cobalt

Technological properties

Property
Application areas

Typical applications include pressure sensor bellows, burn-in and test socket contacts, computer processor socket contacts, and electromagnetic shielding gaskets.