Alloy 165 (C17000) TD04 Rod and Bar

Alternative and trade names
Alloy 165 (C17200) Rod and Bar
Want to keep this datasheet? Save it now in your required format

Description

Alloy 165 rod and bar from Materion Performance Alloys provide strength close to that of Alloy 25, with slightly lower beryllium content. This alloy features high fatigue strength, good electrical and thermal conductivity, as well as resistance to wear, corrosion, galling, and stress relaxation.

Related Standards

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.41 g/cm³

Show Supplier Material materials with Density of 8.41 g/cm³

Dimension

PropertyValueComment

Diameter

0.76 - 76 mm

Show Supplier Material materials with Diameter of 0.76 - 76 mm

Length

91000 mm

Show Supplier Material materials with Length of 91000 mm

max.

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

131 GPa

Show Supplier Material materials with Elastic modulus of 131 GPa

Elongation

23.0 °C

8 - 30 %

Show Supplier Material materials with Elongation of 8 - 30 %

Tensile strength

23.0 °C

590 - 900 MPa

Show Supplier Material materials with Tensile strength of 590 - 900 MPa

Yield strength Rp0.2

23.0 °C

520 - 720 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 520 - 720 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.75E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

Melting point

870 °C

Show Supplier Material materials with Melting point of 870 °C

Thermal conductivity

23.0 °C

105 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 105 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

5.8E-6 - 6.9E-6 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.8E-6 - 6.9E-6 Ω·m

Specific Electrical conductivity

25 - 30 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 25 - 30 % IACS

Chemical properties

PropertyValueComment

Beryllium

1.6 - 1.85 %

Show Supplier Material materials with Beryllium of 1.6 - 1.85 %

Cobalt

0.2 %

Show Supplier Material materials with Cobalt of 0.2 %

min. Nickel + Cobalt

Copper

Balance

Iron

0.6 %

Show Supplier Material materials with Iron of 0.6 %

max., Nickel + Cobalt + Iron

Nickel

0.2 %

Show Supplier Material materials with Nickel of 0.2 %

min. Nickel + Cobalt

Technological properties

Property
Application areas

Typical applications include bushings, bearings and resistance welding components.