Brush Alloy 310 TH04

Alternative and trade names
Brush Alloy 310
Want to keep this datasheet? Save it now in your required format

Description

Materion Performance Alloys’ Brush Alloy 310 is a low cost copper beryllium nickel cobalt alloy with high electrical and thermal conductivity possessing good strength and hardness. The alloy has been shown to have excellent thermal fatigue resistance in use.

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.81 g/cm³

Show Supplier Material materials with Density of 8.81 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

135 GPa

Show Supplier Material materials with Elastic modulus of 135 GPa

Elongation

23.0 °C

10 - 14 %

Show Supplier Material materials with Elongation of 10 - 14 %

Hardness, Rockwell B

23.0 °C

98 [-]

Show Supplier Material materials with Hardness, Rockwell B of 98 [-]

Tensile strength

23.0 °C

720 - 820 MPa

Show Supplier Material materials with Tensile strength of 720 - 820 MPa

Yield strength Rp0.2

23.0 °C

660 - 740 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 660 - 740 MPa

Thermal

PropertyTemperatureValue

Melting point

1030 - 1080 °C

Show Supplier Material materials with Melting point of 1030 - 1080 °C

Thermal conductivity

23.0 °C

235 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 235 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

3.8E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.8E-8 Ω·m

Specific Electrical conductivity

45 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 45 % IACS

Chemical properties

PropertyValue

Beryllium

0.4 - 0.7 %

Show Supplier Material materials with Beryllium of 0.4 - 0.7 %

Cobalt

0.8 - 1.3 %

Show Supplier Material materials with Cobalt of 0.8 - 1.3 %

Copper

Balance

Nickel

0.8 - 1.3 %

Show Supplier Material materials with Nickel of 0.8 - 1.3 %

Technological properties

Property
Application areas

Typical applications include resistance welding electrodes and other welding electrode components. The material also is used for such applications as non-ferrous metal casting dies, plungers and nozzles.