Materion Performance Alloys’ PROtherm alloy is a high conductivity copper mold alloy with good strength. The alloy provides excellent toughness, and the highest conductivity of any alloy with tensile strength in excess of 100,000 psi.

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.83 g/cm³

Show Supplier Material materials with Density of 8.83 g/cm³

Mechanical

PropertyTemperatureValue

Charpy impact energy

23.0 °C

55 J

Show Supplier Material materials with Charpy impact energy of 55 J

Elastic modulus

23.0 °C

138 GPa

Show Supplier Material materials with Elastic modulus of 138 GPa

Elongation

23.0 °C

15 %

Show Supplier Material materials with Elongation of 15 %

Hardness, Rockwell B

23.0 °C

97 [-]

Show Supplier Material materials with Hardness, Rockwell B of 97 [-]

Hardness, Rockwell C

23.0 °C

20 [-]

Show Supplier Material materials with Hardness, Rockwell C of 20 [-]

Tensile strength

23.0 °C

725 MPa

Show Supplier Material materials with Tensile strength of 725 MPa

Yield strength Rp0.2

23.0 °C

620 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 620 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Melting point

1040 °C

Show Supplier Material materials with Melting point of 1040 °C

Specific heat capacity

100.0 °C

410 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 410 J/(kg·K)

Thermal conductivity

100.0 °C

250 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 250 W/(m·K)

Chemical properties

PropertyValue

Beryllium

0.2 - 0.6 %

Show Supplier Material materials with Beryllium of 0.2 - 0.6 %

Copper

Balance

Nickel

1.4 - 2.2 %

Show Supplier Material materials with Nickel of 1.4 - 2.2 %

Technological properties

Property
Application areas

PROtherm alloy is used as blow mold cavities, injection mold cores and cavities and hot runners.