Alloy 3 (C17510) TB00 Forging and Extrusion

Want to keep this datasheet? Save it now in your required format

Description

Alloy 3 from Materion Performance Alloys provides high electrical and thermal conductivity coupled with moderate strength.

Related Standards

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.83 g/cm³

Show Supplier Material materials with Density of 8.83 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

138 GPa

Show Supplier Material materials with Elastic modulus of 138 GPa

Elongation

23.0 °C

20 - 35 %

Show Supplier Material materials with Elongation of 20 - 35 %

Hardness, Rockwell B

23.0 °C

20 - 50 [-]

Show Supplier Material materials with Hardness, Rockwell B of 20 - 50 [-]

Tensile strength

23.0 °C

240 - 380 MPa

Show Supplier Material materials with Tensile strength of 240 - 380 MPa

Yield strength Rp0.2

23.0 °C

130 - 280 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 130 - 280 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.76E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.76E-5 1/K

Melting point

1040 °C

Show Supplier Material materials with Melting point of 1040 °C

Thermal conductivity

23.0 °C

240 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 240 W/(m·K)

Electrical

PropertyValue

Specific Electrical conductivity

45 - 60 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 45 - 60 % IACS

Chemical properties

PropertyValue

Beryllium

0.2 - 0.6 %

Show Supplier Material materials with Beryllium of 0.2 - 0.6 %

Copper

Balance

Nickel

1.4 - 2.2 %

Show Supplier Material materials with Nickel of 1.4 - 2.2 %

Technological properties

Property
Application areas

Typical applications for parts finished by forging or extrusion of these alloys include continuous casting mold components and resistance welding components.