EtchMetᵀᴹ (C17200) TH04 Wire

Want to keep this datasheet? Save it now in your required format

Description

EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. These devices have a relatively large mass (lense) suspended by extremely small, thin springs. The small size of the springs requires very high strength material to withstand shock loads when the phone is dropped or deliberately tapped against an NFC reader. Therefore, the springs must be made from a very robust material. Furthermore, the lack of a damping mechanism makes high spring stiffness important to combat vibration. EtchMet wire provides a number of advantages that make it the ideal material for this application:


  • It has a uniform elastic modulus across all thicknesses/diameters and from product form to product form. This provides consistent stiffness and damping behavior which makes spring calculations easy.
  • It has a very high resilience allowing it to withstand impact loads without fracturing or permanently deforming.
  • It has high fatigue strength to withstand many drops and actuation cycles.
  • It solders and welds readily.
  • Related Standards

    This material data has been provided by Materion Brush GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.3 - 8.36 g/cm³

    Show Supplier Material materials with Density of 8.3 - 8.36 g/cm³

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    131 GPa

    Show Supplier Material materials with Elastic modulus of 131 GPa

    Elongation

    23.0 °C

    1 %

    Show Supplier Material materials with Elongation of 1 %

    min., for wire with 0.1mm diameter and more.

    Tensile strength

    23.0 °C

    1340 - 1590 MPa

    Show Supplier Material materials with Tensile strength of 1340 - 1590 MPa

    Yield strength Rp0.2

    23.0 °C

    1240 - 1520 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 1240 - 1520 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    1.75E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

    Thermal conductivity

    23.0 °C

    105 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 105 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical resistivity

    23.0 °C

    6.2E-6 - 7.8E-6 Ω·m

    Show Supplier Material materials with Electrical resistivity of 6.2E-6 - 7.8E-6 Ω·m

    Specific Electrical conductivity

    22 - 28 % IACS

    Show Supplier Material materials with Specific Electrical conductivity of 22 - 28 % IACS

    Magnetic

    PropertyTemperatureValueComment

    Relative magnetic permeability

    23.0 °C

    1 [-]

    Show Supplier Material materials with Relative magnetic permeability of 1 [-]

    max.

    Chemical properties

    PropertyValueComment

    Beryllium

    1.8 - 2 %

    Show Supplier Material materials with Beryllium of 1.8 - 2 %

    Cobalt

    0.2 %

    Show Supplier Material materials with Cobalt of 0.2 %

    min. Nickel + Cobalt

    Copper

    Balance

    Iron

    0.6 %

    Show Supplier Material materials with Iron of 0.6 %

    max. Nickel + Cobalt + Iron

    Nickel

    0.2 %

    Show Supplier Material materials with Nickel of 0.2 %

    min. Nickel + Cobalt

    Technological properties

    Property
    Application areas

    EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras.