E-60 Beryllium

Want to keep this datasheet? Save it now in your required format

Description

Beryllium and beryllium oxide metal matrix composites provide outstanding stiffness-to-weight ratios with thermal cycle reliability over a broad temperature range. The high elastic modulus of helps absorb vibrations, lowering the material fatigue of attached modules and wire bonds.


E-Materials offer high thermal conductivity and low thermal expansion. Their thermal expansion can be adjusted to match that of other materials, such as silicon, gallium arsenide and various ceramics. Features include:


  • Low weight - density
  • High strength
  • High modulus
  • Excellent thermal expansion
  • Excellent thermal conductivity

  • This material data has been provided by Materion Brush GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    2.51 g/cm³

    Show Supplier Material materials with Density of 2.51 g/cm³

    Mechanical

    PropertyTemperatureValue

    Elastic modulus

    23.0 °C

    313 GPa

    Show Supplier Material materials with Elastic modulus of 313 GPa

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    6.5E-6 - 7.9E-6 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 6.5E-6 - 7.9E-6 1/K

    ASTM E228, ASTM E289

    Specific heat capacity

    23.0 °C

    5275 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 5275 J/(kg·K)

    Thermal conductivity

    23.0 °C

    210 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 210 W/(m·K)

    Thermal diffusivity

    23.0 °C

    15.84 mm²/s

    Show Supplier Material materials with Thermal diffusivity of 15.84 mm²/s

    Chemical properties

    PropertyValue

    Beryllium

    BeO: 69.4-73.2%

    Technological properties

    Property
    Application areas

    Microelectronics - electronic heat sinks and chill plates, Aerospace - aerospace applications and components, Semiconductor - power devices