BS C109 Tellurium Copper

View suppliers (10)
Want to keep this datasheet? Save it now in your required format

Description

2.1545 (CuTeP) is a free-machining grade of copper with an addition of around 0.5% tellurium. The tellurium content raises the machinability rating to 90% with minimal effect on conductivity and ductility. C109 has freedom from hydrogen embrittlement, enabling the use of this grade in electrical and electronic applications where accuracy and intricacy are required. It shows the following features and properties:


  • Enhanced strength levels over standard copper
  • Retention of properties at elevated temperatures
  • Outstanding machining qualities
  • Excellent electrical and thermal conductivity
  • Freedom from hydrogen embrittlement
  • Good hot and cold workability
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Chemical properties

    PropertyValue

    Copper

    99 %

    Show Material materials with Copper of 99 %

    Tellurium

    0.5 %

    Show Material materials with Tellurium of 0.5 %

    Technological properties

    Property
    Application areas

    General: Transformer and circuit breaker terminals, contacts, connectors, clamps, bolts, nuts, studs and other high current-carrying components requiring free machinability

    Cold Forming

    Good cold workability

    General machinability

    Outstanding machining

    Hot forming

    Good hot workability