2.0872 (CuNi10Fe1Mn) cupronickel is a 90% copper, 10% nickel alloy that also contains small but important additions of iron and manganese to enhance overall strength corrosion resistance. This, combined with high ductility and toughness, makes it a popular grade for marine, architectural and industrial applications. It shows the following features and properties:


  • High ductility and toughness
  • Excellent resistance to erosion and corrosion in seawater
  • Inherent resistance to biofouling
  • Excellent fabrication and welding properties
  • Retention of mechanical properties down to cryogenic temperatures
  • Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Mechanical

    PropertyTemperatureValue

    Elongation

    23.0 °C

    27 - 30 %

    Show Material materials with Elongation of 27 - 30 %

    Hardness, Brinell

    23.0 °C

    70 - 120 [-]

    Show Material materials with Hardness, Brinell of 70 - 120 [-]

    Tensile strength

    23.0 °C

    280 - 310 MPa

    Show Material materials with Tensile strength of 280 - 310 MPa

    Yield strength Rp0.2

    23.0 °C

    105 MPa

    Show Material materials with Yield strength Rp0.2 of 105 MPa

    Chemical properties

    PropertyValue

    Copper

    Balance

    Iron

    1.5 %

    Show Material materials with Iron of 1.5 %

    Manganese

    0.75 %

    Show Material materials with Manganese of 0.75 %

    Nickel

    10.5 %

    Show Material materials with Nickel of 10.5 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Salt water pipes and fittings, hot water tanks, salt water baffles, propeller sleeves, valve and pump components, flanges, boat hulls, marine fittings and marine hardware;Chemical processing: Heat exchanger and cooling plant, evaporator tubes, pump and valve trim;Other: Power steering tube, brake lines, condenser plates, pressure vessels and distiller tubes

    Corrosion properties

    Excellent resistance to erosion and corrosion in seawater.

    General machinability