Carbon Chopped Fibre (C006560)

Alternative and trade names
Grafil 34-700 carbon fiber
Want to keep this datasheet? Save it now in your required format

Description

Carbon - Chopped Fibre - C 006560 is a high strength, PAN based fiber

Related Standards

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.8 g/cm³

Show Material materials with Density of 1.8 g/cm³

SRM 15 (typical fibre properties)

Yield 12K

23.0 °C

800 mg/m

Show Material materials with Yield 12K of 800 mg/m

SRM 13

Yield 24K

23.0 °C

1600 mg/m

Show Material materials with Yield 24K of 1600 mg/m

SRM 13

Dimension

PropertyValueComment

Diameter

7E-3 mm

Show Material materials with Diameter of 7E-3 mm

Length

6 mm

Show Material materials with Length of 6 mm

fiber length

Mechanical

PropertyTemperatureValueComment

Compressive modulus

23.0 °C

127 MPa

Show Material materials with Compressive modulus of 127 MPa

ASTM D3039

Compressive modulus, transverse

23.0 °C

10.2 MPa

Show Material materials with Compressive modulus, transverse of 10.2 MPa

ASTM D3039

Compressive strength

23.0 °C

1365 MPa

Show Material materials with Compressive strength of 1365 MPa

ASTM D3039

Compressive strength, transverse

23.0 °C

196 MPa

Show Material materials with Compressive strength, transverse of 196 MPa

ASTM D3039

Elastic modulus

23.0 °C

137 GPa

Show Material materials with Elastic modulus of 137 GPa

ASTM D3039

Elastic modulus, transverse

23.0 °C

9.2 GPa

Show Material materials with Elastic modulus, transverse of 9.2 GPa

ASTM D3039

Flexural modulus

23.0 °C

132 GPa

Show Material materials with Flexural modulus of 132 GPa

ASTM D790 (L/D=32, Vf=61%)

Flexural modulus, transverse

23.0 °C

8.8 GPa

Show Material materials with Flexural modulus, transverse of 8.8 GPa

ASTM D790 (L/D=32, Vf=61%)

Flexural strength

23.0 °C

1745 MPa

Show Material materials with Flexural strength of 1745 MPa

ASTM D790 (L/D=32, Vf=61%)

Flexural strength, transverse

23.0 °C

102 MPa

Show Material materials with Flexural strength, transverse of 102 MPa

ASTM D790 (L/D=32, Vf=61%)

Interlaminar shear strength

23.0 °C

97 MPa

Show Material materials with Interlaminar shear strength of 97 MPa

ASTM D2344 (L/D=4, Vf=59%)

Tensile strength

23.0 °C

2572 MPa

Show Material materials with Tensile strength of 2572 MPa

ASTM D3039

Tensile strength, transverse

23.0 °C

81 MPa

Show Material materials with Tensile strength, transverse of 81 MPa

ASTM D3039

Tow tensile modulus

23.0 °C

234 GPa

Show Material materials with Tow tensile modulus of 234 GPa

SRM 16 (typical fibre properties)

Tow tensile strength

23.0 °C

4830 MPa

Show Material materials with Tow tensile strength of 4830 MPa

SRM 16 (typical fibre properties)

Technological properties

Property
Processing history

Epoxy sized 1.2%