Description

Standard properties of manufactured graphite include thermal stability, thermal conductivity, natural lubricity and chemical resistance to fluids. Flexible graphite combines these properties with the added characteristics of flexibility, compatibility, conformability and resilience. These characteristics differentiate flexible graphite from other forms of graphite, making it a superior, high-performance sealing material.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

1.12 g/cm³

Show Material materials with Bulk density of 1.12 g/cm³

ASTM F-1315

Oxidation rate

500.0 °C

0.75 g/m²·h

Show Material materials with Oxidation rate of 0.75 g/m²·h

700.0 °C

130 g/m²·h

Show Material materials with Oxidation rate of 130 g/m²·h

Mechanical

PropertyTemperatureValueComment

Compressive modulus

23.0 °C

190 MPa

Show Material materials with Compressive modulus of 190 MPa

Compressive strength

23.0 °C

165 MPa

Show Material materials with Compressive strength of 165 MPa

ASTM C-695

Tensile strength

23.0 °C

5.2 MPa

Show Material materials with Tensile strength of 5.2 MPa

ASTM F-152

Tow tensile strength

23.0 °C

190 MPa

Show Material materials with Tow tensile strength of 190 MPa

Thermal

PropertyValue

Max service temperature

3000 °C

Show Material materials with Max service temperature of 3000 °C

Min service temperature

-240 °C

Show Material materials with Min service temperature of -240 °C

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

8E-8 Ω·m

Show Material materials with Electrical resistivity of 8E-8 Ω·m

ASTM C-611

Chemical properties

PropertyValueComment

Carbon

99.9 %

Show Material materials with Carbon of 99.9 %

ASTM C-695

Chlorine

5E-3 %

Show Material materials with Chlorine of 5E-3 %

ASTM F-1277 (maximum leachable chlorides)

Sulfur

0.045 %

Show Material materials with Sulfur of 0.045 %

Leco Method

Technological properties

Property
Application areas

Flexible Graphite has unique physical and chemical properties that make it ideal for sealing and for high-temperature applications, such as thermal radiation shielding. Flexible graphite is a distinctive material with the essential characteristics of graphite plus some unique properties which make it a valuable material for packings and gaskets.