Easy Transfer Monolayer Graphene on Polymer Film

Want to keep this datasheet? Save it now in your required format

Description

“Easy Transfer”: the easiest way to transfer monolayer graphene onto your substrate. The growth method was CVD synthesis.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Grain size

20 μm

Show Material materials with Grain size of 20 μm

Dimension

PropertyValueComment

Thickness

3.45E-7 mm

Show Material materials with Thickness of 3.45E-7 mm

theoretical thickness of graphene monolayer

Electrical

PropertyTemperatureValueComment

Carrier mobility

23.0 °C

3760 cm²/Vs

Show Material materials with Carrier mobility of 3760 cm²/Vs

FET Electron Mobility on SiO₂/Si substrate

Surface resistivity

23.0 °C

410 - 490 Ω/sq

Show Material materials with Surface resistivity of 410 - 490 Ω/sq

Van der Pauw sheet resistance on SiO₂/Si substrate (1cm x 1cm)

Optical

PropertyValue

Luminous transmittance

97 [-]

Show Material materials with Luminous transmittance of 97 [-]

Technological properties

Property
Application areas

Graphene research, flexible batteries, electronics, aerospace industry, MEMS and NEMS, microactuators, conductive coatings

Other

"Easy Transfer": avoids metal etching, avoids hazardous chemical handling, bottom layer removed. Coverage of >98%.

Processing history

Growth method: CVD. Processed in Clean Room Class 1000.