Pyrolytic graphite (PG) is a unique form of graphite manufactured by decomposition of hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is near theoretical density and extremely anisotropic.


As an example, PG exhibits thermal conductivity consistent with the best conductors in the “ab” plane and lower than alumina brick in the “c” direction. Mechanical, thermal, and electrical properties are generally far superior to conventional graphites.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.18 - 2.2 g/cm³

Show Material materials with Density of 2.18 - 2.2 g/cm³

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

100 MPa

Show Material materials with Compressive strength of 100 MPa

Elastic modulus

23.0 °C

20 GPa

Show Material materials with Elastic modulus of 20 GPa

Flexural strength

23.0 °C

120 MPa

Show Material materials with Flexural strength of 120 MPa

Tensile strength

23.0 °C

80 MPa

Show Material materials with Tensile strength of 80 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5E-7 1/K

Show Material materials with Coefficient of thermal expansion of 5E-7 1/K

Coefficient of thermal expansion, transverse

23.0 °C

2E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 2E-5 1/K

Max service temperature

3000 °C

Show Material materials with Max service temperature of 3000 °C

Melting point

3650 °C

Show Material materials with Melting point of 3650 °C

sublimation

Thermal conductivity

23.0 °C

300 W/(m·K)

Show Material materials with Thermal conductivity of 300 W/(m·K)

Thermal conductivity, through-plane

23.0 °C

3.5 W/(m·K)

Show Material materials with Thermal conductivity, through-plane of 3.5 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

5E-6 Ω·m

Show Material materials with Electrical resistivity of 5E-6 Ω·m

Electrical resistivity, transverse

23.0 °C

5E-3 Ω·m

Show Material materials with Electrical resistivity, transverse of 5E-3 Ω·m

Technological properties

Property
Application areas

Sputtering Targets, Ion Beam Grids, Ion Implant Hardware, Liquid Phase Epitaxy Hardware, Crucibles for Ultra High Vacuum, Thermal Insulators, Rocket Nozzles, Heater Elements

Other

The key features are: Chemically inert, high purity, stable to 3000°C, impermeable, directional electrical & thermal characteristics, self- lubricating, nondusting, low etch rate