Rayon Graphite Felt

Want to keep this datasheet? Save it now in your required format

Description

Graphite Felts is a high quality insulation for vacuum and inert gas furnaces where the maximum temperature can be up to 3000°C.


Rayon Graphite Felt is the ideal choice for vacuum furnaces or process temperatures above 2000°C due to its low shrinkage and negligible gas evolution below 3000°C.


Rayon Graphite Felt also features enhanced oxidation resistance. For special requirements, it can be purified to less than 10 ppm in total ash content.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Tensile strength

23.0 °C

0.15 MPa

Show Material materials with Tensile strength of 0.15 MPa

Thermal

PropertyTemperatureValueComment

Max service temperature

3000 °C

Show Material materials with Max service temperature of 3000 °C

in vacuum

Max service temperature, inert

3600 °C

Show Material materials with Max service temperature, inert of 3600 °C

Thermal conductivity

1000.0 °C

0.4 W/(m·K)

Show Material materials with Thermal conductivity of 0.4 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.4E-3 Ω·m

Show Material materials with Electrical resistivity of 1.4E-3 Ω·m

Chemical properties

PropertyValue

Carbon

99.96 %

Show Material materials with Carbon of 99.96 %

Technological properties

Property
Application areas

Vacuum and High Pressure Sintering Industry: Heat Insulation for Metal Sintering, Non Oxide Ceramics, Tungsten Carbide manufacturing; Vacuum Treatment Industry: Heat Insulation for Commercial Heat Treat Furnaces, Hardening, Tempering, etc. Crystal Growing Industry: Heat Insulation for silicon, Sic, Indium phosphide, Gallium Arsenide, Sapphire, Optical Crystals, Solar Ingots; Special Casting Industry: Heat Insulation for precision casting of DS/SC turbine engine components and Metal Matrix Composites.Graphitizing/CVD Applications: Heat Insulation for High Modulus Carbon Fiber Production, Halogen purification Furnaces; Electronic/Semiconductor Industry: Heat Insulation for Materials for various precursor applications; Aerospace Industry: Hot isostatic process furnaces, heat treating, sintering, brazing furnaces, autoclaves; Solar cells: graphite felt electrode in the vanadium redox flow battery. Filtering materials of scorching gas, liquid and fused metal; Perforated electrode of fuel battery, Catalyst carrier; Face of corrosion resistant materials; Semi-Conductor: as insulation boards and cylinders using together with high purified graphite crucibles, heating elements and other elements within the hot zone; As the raw materials for producing Rigid Felt boards; The 2.5 mm - 3 mm thick rayon graphite felt to be cut into strips as the light and heat filament in “BATHROOMMASTER” and “Quartz tube heating lamp”; Furnace - resistance or induction heated vacuum furnaces and inert gas furnaces, such as degassing furnaces, brazing furnaces, soft and bright annealing furnaces, sintering furnaces for hard metals, carburizing furnaces, laboratory graphitizing furnaces; inductively heated melting and heat treatment furnaces, in which a proportion of the ceramic insulating material is replaced by felt in order to increase the electrical efficiency and prevent the liquid metal from coming into contact with the induction coil in the event of crucible fracture (no wetting); Thermal insulation, as filters, and as catalyst support; Porous electrodes and Turbine blade manufacturing