Graphene Powder is obtained in proprietary plasma reactors by cracking greenhouse gases, such as methane and carbon dioxide, using advanced microwave plasma chemistry. This process ensures that the Graphene Powder has no additive, surfactant, catalyst or metal impurities. This Green process is taking place by converting methane, a greenhouse gas that is a harmful by-product of ubiquitous processes like farming, landfills and palm oil milling.


The great electrical conductivity, thermal conductivity and mechanical strength of this product has proven to be an important feature in research and development of a wide range of applications spanning power supply, aviation, automotive, construction etc.


These Green Graphene nanoplatelets are very thin and slightly crumpled and they do not stack, ensuring optimal electrical, thermal and mechanical performance. Thus, this product is an extremely good nanofiller suitable for electronic inks, polymers, metal composites and coating.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Bulk density

23.0 °C

0.18 - 0.2 g/cm³

Show Material materials with Bulk density of 0.18 - 0.2 g/cm³

Flake thickness

43470 nm

Show Material materials with Flake thickness of 43470 nm

Lateral flake size

250 - 550 nm

Show Material materials with Lateral flake size of 250 - 550 nm

Layer number

3 - 15 [-]

Show Material materials with Layer number of 3 - 15 [-]

Pore volume

0.06 cm³/g

Show Material materials with Pore volume of 0.06 cm³/g

Specific surface area

125 - 135 m²/g

Show Material materials with Specific surface area of 125 - 135 m²/g

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

900 - 1050 S/m

Show Material materials with Electrical conductivity of 900 - 1050 S/m

Chemical properties

PropertyValue

Carbon

98.9 - 99.1 %

Show Material materials with Carbon of 98.9 - 99.1 %

Hydrogen

0.68 - 0.72 %

Show Material materials with Hydrogen of 0.68 - 0.72 %

Nitrogen

0.16 - 0.28 %

Show Material materials with Nitrogen of 0.16 - 0.28 %

Oxygen

0.55 - 0.57 %

Show Material materials with Oxygen of 0.55 - 0.57 %

Technological properties

Property
Processing history

No catalyst impurities