Multi Wall Carbon Nanotubes “Chunky” Powder NC006060 (>90% purity)

Want to keep this datasheet? Save it now in your required format

Description

Free Standing aligned CNT arrays (Carpets) are synthesized by floating catalyst CVD method within a horizontal quartz reaction tube.


The CNT synthesis parameters are carefully selected to provide maximum-yield of CNT growth, high packing density as well as high graphitization level.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Graphitization level

0.3 - 0.4 [-]

Show Material materials with Graphitization level of 0.3 - 0.4 [-]

Dimension

PropertyValue

Nanotube diameter

30 - 90 nm

Show Material materials with Nanotube diameter of 30 - 90 nm

Nanotube length

300 - 1000 µm

Show Material materials with Nanotube length of 300 - 1000 µm

Thermal

PropertyValue

Oxidation threshold

600 - 700 °C

Show Material materials with Oxidation threshold of 600 - 700 °C