General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 4.45 g/cm³ Show Material materials with Density of 4.45 g/cm³ | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Dimension
Property | Value | Related Standards | Shape |
---|---|---|---|
Diameter | 5 mm Show Material materials with Diameter of 5 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
25.4 mm Show Material materials with Diameter of 25.4 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet | |
125 mm Show Material materials with Diameter of 125 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet | |
130 mm Show Material materials with Diameter of 130 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube | |
Length | 1000 mm Show Material materials with Length of 1000 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
5000 mm Show Material materials with Length of 5000 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet |
Mechanical
Property | Value | Related Standards | Shape |
---|---|---|---|
Elastic modulus | 110.0 GPa Show Material materials with Elastic modulus of 110.0 GPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Tensile strength | 825.0 - 860.0 MPa Show Material materials with Tensile strength of 825.0 - 860.0 MPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Yield strength | 760.0 MPa Show Material materials with Yield strength of 760.0 MPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Thermal
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Coefficient of thermal expansion of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Melting point | 1500.0 - 1750.0 °C Show Material materials with Melting point of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | ||
Specific heat capacity | 560 J/(kg·K) Show Material materials with Specific heat capacity of 560 J/(kg·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube | |
Thermal conductivity | 6.9 W/(m·K) Show Material materials with Thermal conductivity of 6.9 W/(m·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Carbon | 0.08 Show Material materials with Carbon of 0.08 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Iron | 0.25 Show Material materials with Iron of 0.25 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Oxygen | 0.13 Show Material materials with Oxygen of 0.13 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |