Chloroprene rubber (CR)

Alternative and trade names
Baypren®, Denka™, Skyprene®, Neoprene®
Want to keep this datasheet? Save it now in your required format

Description

Chloroprene rubber demonstrates a good balance of features, including such as resistance to ozone, oil and heat; flame retardancy, weatherability, special cohesiveness, etc., and is very easy to process.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.15 - 1.5 g/cm³

Show Material materials with Density of 1.15 - 1.5 g/cm³

Mechanical

PropertyValueComment

Elongation

100.0 - 900.0 %

Show Material materials with Elongation of 100.0 - 900.0 %

Tensile strength

4.0 - 25.0 MPa

Show Material materials with Tensile strength of 4.0 - 25.0 MPa

at 100-900% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.00014 - 0.00025 1/K

Show Material materials with Coefficient of thermal expansion of 0.00014 - 0.00025 1/K

Specific heat capacity

2200 J/(kg·K)

Show Material materials with Specific heat capacity of 2200 J/(kg·K)

Thermal conductivity

0.15 - 0.2 W/(m·K)

Show Material materials with Thermal conductivity of 0.15 - 0.2 W/(m·K)

Electrical

PropertyValue

Dielectric constant

5 [-]

Show Material materials with Dielectric constant of 5 [-]

9 [-]

Show Material materials with Dielectric constant of 9 [-]

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Bellows, grommets, cooling water hoses, roofing materials, conveyer belts

Processing methods

Compression molding, extrusion, vulcanization