General
Property | Value |
---|---|
Density | 0.906 - 1.49 g/cm³ Show Material materials with Density of 0.906 - 1.49 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 100.0 - 900.0 % Show Material materials with Elongation of 100.0 - 900.0 % | |
Tensile strength | 4.0 - 35.0 MPa Show Material materials with Tensile strength of 4.0 - 35.0 MPa | at 100-900% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.00018 - 0.00026 1/K Show Material materials with Coefficient of thermal expansion of 0.00018 - 0.00026 1/K |
Specific heat capacity | 1400.0 - 2100.0 J/(kg·K) Show Material materials with Specific heat capacity of 1400.0 - 2100.0 J/(kg·K) |
Thermal conductivity | 0.13 - 0.28 W/(m·K) Show Material materials with Thermal conductivity of 0.13 - 0.28 W/(m·K) |
Electrical
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Springs, truck tires, cutting gaskets, washers | |