Natural rubber (NR)

Want to keep this datasheet? Save it now in your required format

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

0.906 - 1.49 g/cm³

Show Material materials with Density of 0.906 - 1.49 g/cm³

Mechanical

PropertyValueComment

Elongation

100.0 - 900.0 %

Show Material materials with Elongation of 100.0 - 900.0 %

Tensile strength

4.0 - 35.0 MPa

Show Material materials with Tensile strength of 4.0 - 35.0 MPa

at 100-900% strain

Thermal

PropertyValueComment

Coefficient of thermal expansion

0.00018 - 0.00026 1/K

Show Material materials with Coefficient of thermal expansion of 0.00018 - 0.00026 1/K

Max service temperature

120 °C

Show Material materials with Max service temperature of 120 °C

Short

70.0 - 90.0 °C

Show Material materials with Max service temperature of 70.0 - 90.0 °C

Long

Specific heat capacity

1400.0 - 2100.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1400.0 - 2100.0 J/(kg·K)

Thermal conductivity

0.13 - 0.28 W/(m·K)

Show Material materials with Thermal conductivity of 0.13 - 0.28 W/(m·K)

Electrical

PropertyValue

Dielectric constant

2.37 [-]

Show Material materials with Dielectric constant of 2.37 [-]

3 [-]

Show Material materials with Dielectric constant of 3 [-]

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Springs, truck tires, cutting gaskets, washers

Processing methods

Compression molding, extrusion, vulcanization